ddgarcia05
Member
- Joined
- Feb 27, 2014
- Messages
- 114
I have a harbor freight dual rotary tumbler with one pound of SS pins, one pound of brass, water, a generous amount of dawn and what I think is a generous amount if lemishine.
The first shiny group is was in the first container (4 hrs), second group was tumbled 8 hours, third group was over 12 hours. (3rd group also done with the first one but with different result)
Why are none as shiny as the first group? To much soap? Lemishine?
The first shiny group is was in the first container (4 hrs), second group was tumbled 8 hours, third group was over 12 hours. (3rd group also done with the first one but with different result)
Why are none as shiny as the first group? To much soap? Lemishine?